高温高压蒸汽灭菌对不锈钢根管器械循环疲劳性能的影响

赵渤锐1,胡欣2,吴卉1,陈阵1,李长义2   

  1. 1. 天津医科大学口腔医院
    2. 天津医大口腔医院
  • 收稿日期:2014-02-14 修回日期:2014-06-06 出版日期:2014-10-15 发布日期:2014-10-15
  • 通讯作者: 赵渤锐

The Effect of Steam Sterilization on Cyclic Fatigue of Stainless Steel Files

  • Received:2014-02-14 Revised:2014-06-06 Published:2014-10-15 Online:2014-10-15
  • Contact: ZHAO Bo rui

摘要:

【摘要】目的 研究高温高压蒸汽灭菌过程对不锈钢根管预备器械循环疲劳性的影响。方法 选取25#不锈钢K 锉50 支,随机分为5 组,每组10 支。其中1 组作为空白对照组,2~5 组分别经1 次、3 次、4 次、5 次高温高压蒸汽灭菌后,利用自制循环疲劳性能测试设备测得循环疲劳断裂次数。采用扫描电镜分析折断试样断口的显微结构。结果 1~5 组的转数分别为4 345.2±384.2、3 937.9±645.4、3 812.9±532.5、3 626.2±380.0、3 625.9±565.6,5 组比较差异有统计学意义(F=2.598,P<0.05)。4 组、5 组经4 次及5 次后循环疲劳性能较1 组明显降低(P < 0.05)。1 组、2 组试样的断口为韧性断口,断口表面均匀分布着大量规整、较深的韧窝,且可以清晰看见断裂时形成的微观空洞。4 组试样在出现韧性断口韧窝结构的同时可见脆性延晶断裂的断口形貌,其特征为出现薄片状脆性沉淀相,晶界面清洁、光滑,界面棱角清晰,多面立体感强。结论 经过4 次以上高温高压蒸汽灭菌后,25#不锈钢K 型锉的循环疲劳性能降低,存在潜在的折断风险。

关键词: 不锈钢, 蒸汽, 灭菌, 根管疗法, 牙科器械, 循环疲劳性能

Abstract:

[Abstract] Objective  Comparing the effects of steam sterilization on cyclic fatigue of stainless steel files.  Meth ods  Fifty instruments of 25# stainless steel K files were randomly divided into 5 groups, which include 10 in each group. Group 1 was the blank control group, group 2 to 5 were subjected to 1, 3, 4, 5 steam sterilization cycles, then the files were tested by a custom-made device to assess cyclic fatigue and the number of cycles of failure (NCF) was calculated. Microstructure of each file’s fracture surface was analyzed by Scanning Electron microscope (SEM). Results  NCF in the 5 groups were 4 345.2±384.2,3 937.9±645.4,3 812.9±532.5,3 626.2±380.0,3 625.9±565.6 respectively, and the differences among 5 groups were significantly different(F=2.598, P < 0.05). After 4 or 5 times of steam sterilization, cyclic fatigue decreased if compared with that in control group (P < 0.05). Fracture surface in group 1 and group 2 was tough dimple structure and large numbers of regular, deep dimples were distributed on the surface. You could also see micro cavities clearly formed by fracture; Fracture surface in group 4 was dimple structure in brittle intergranular morphology. It is characterized by the presence of thin brittle precipitates, clean and smooth crystal interface, and a great sense of polyhedral stereo. Conclusion  After 4 times of steam sterilization, cyclic fatigue strength of 25# stainless steel K files declined, which possessed the poten? tial risk of fracture.

Key words: stainless steel, steam, sterilization, root canal therapy, dental instruments, dental instruments